Case studies / Paint protection film (PPF)

PPF top coat: ΔE 0.8 where the incumbent measured 4.2

A paint protection film top coat compared against its incumbent catalyst in the same accelerated aging run.

Paint protection film (PPF)PPF & CoatingsPC-42 · PC-50
Result at a glance
ΔE 0.8
after 85°C / 48 h accelerated aging
Zero yellowing
visual assessment after aging
Optical clarity
mirror gloss retained

Each figure is tied to a measurement, and the result section below states the conditions that produced it. Field data and accelerated aging data are labelled separately, and the disclosure at the end of the case states how the data was obtained.

Visualised

Measured, not claimed.

Schematic of the measurement behind this case: the same conditions, drawn to be read at a glance. The drawing is illustrative; the measured values are the ones stated in the result sections.

85 °C / 48 h accelerated aging: ΔE 4.2 versus ΔE 0.8ACCELERATED AGING · 85 °C / 48 H · SAME TEST RUNCONVENTIONAL KARSTEDTΔE 4.2VISIBLE YELLOWINGPC-42 · ANTI-YELLOWINGΔE 0.8NO VISIBLE COLOUR SHIFTVS80–120 °C cure window · 0.05–0.5 % dosage · PC-611 / PC-612 inhibitor
Accelerated aging comparison: ΔE 4.2 with a conventional Karstedt's catalyst against ΔE 0.8 with PC-42, both run in the same 85 °C / 48 h test and measured against an unstressed reference film. Colour patches are illustrative; the ΔE values are the measured results.
On the line

Where this grade is used.

Representative production images of the processes these grades are specified for. The parts shown are end applications, not test data; measured values stay in the data sections above.

Coating head applying a clear liquid top coat onto a roll of film
Clear top coat on automotive filmA transparent top coat is laid on the moving film by a coating head. Cure speed and colour stability after 85 °C / 48 h are the two acceptance points at this step.
01 / Challenge

The challenge.

A TPU paint protection film yellowed within the warranty period under combined solar UV and engine heat. The incumbent catalyst measured ΔE 4.2 after 48 h at 85°C — visible to the eye and outside specification.

The incumbent was tested in the same run, which is what makes the two ΔE figures directly comparable. Running both catalysts under one set of oven conditions removes the batch-to-batch variation that makes separate tests hard to read.

The film's failure is cosmetic first and functional later: customers see the colour change before they measure it, and the specification is written in ΔE because visual judgement does not hold across suppliers.

02 / Solution

The solution.

PC-42 anti-yellowing catalyst in the top coat, with PC-611 inhibitor for line stability on the slot-die coater.

Dosage stayed inside the normal 0.05%–0.5% window. The change was the grade, not the loading: colour retention comes from the catalyst chemistry, and adding more of a conventional catalyst does not buy the same result.

PC-611 kept the slot-die bath stable through the run. On a coating line the inhibitor is part of the colour result, because a change in working time changes coat weight and therefore the optical path of the film.

03 / Result

The result, and what produced it.

The numbers at the top of the page are the headline metrics from this case. The paragraphs here explain what produced them, with the test method and the exposure stated alongside.

The reformulated top coat measured ΔE 0.8 after 85°C / 48 h against 4.2 for the incumbent, with no visible yellowing and mirror gloss retained in the customer's assessment. Colour difference was measured against an unstressed reference film.

The result is an accelerated-aging comparison with customer line validation. It is a screening result for formulation decisions, not a prediction of warranty life or field durability.

Accelerated aging accelerates one mechanism; it cannot reproduce every combination of UV dose, heat cycling and chemical exposure a film meets in service. Use the ΔE comparison to choose a grade, then validate on the vehicle programme's own cycle.

Test conditions and data scope

Accelerated aging at 85°C for 48 h, colour difference measured against unstressed reference film; comparison catalyst tested in the same run.

Internal accelerated aging comparison, with customer line validation.

Traceability

The grades and the application behind this case.

Every case is tied to a catalyst grade and to an application page. The grade page carries the full specification; the application page carries the process window, dosage range and inhibitor pairing for this class of part.

ModelPt concentrationViscosityRecommended dosage
PC-425,000 PPM300–500 cP0.05%–0.5% of total compound
PC-50Custom (1,000–20,000 PPM)5–50 cP0.05%–0.5% of total compound

Open a model for packaging, shelf life, features and inhibitor pairing. Where a case names more than one grade, the solution section states which one was used in the reported trial.

Application

PPF & Coatings

Zero yellowing under engine heat and solar UV.

Optical-grade platinum catalysis for TPU and PET paint protection film top coats and adhesive modification.

PC-42PC-50PC-51
Next step

Run a comparable trial on your own line.

Send the part, the failure and the acceptance test. We will send evaluation samples of the grade used in this case, paired with the matching inhibitor, and confirm the starting dosage for your cure window.

Technical reply within 24 hours
Evaluation samples in 5–7 days
COA, TDS and SDS on request
Custom concentration 1,000–20,000 PPM