Mini LED encapsulation: 99.82% transmittance at 95% yield
A high-refractive-index encapsulation compound that clouded when the catalyst was added, measured by transmittance after cure and by production yield.
Each figure is tied to a measurement, and the result section below states the conditions that produced it. Field data and accelerated aging data are labelled separately, and the disclosure at the end of the case states how the data was obtained.
Measured, not claimed.
Schematic of the measurement behind this case: the same conditions, drawn to be read at a glance. The drawing is illustrative; the measured values are the ones stated in the result sections.
Where this grade is used.
Representative production images of the processes these grades are specified for. The parts shown are end applications, not test data; measured values stay in the data sections above.

The challenge.
A high-refractive-index encapsulation compound clouded when the catalyst was added, and the resulting light scattering failed the transmittance target. Yield was limited by optical rejects rather than by the dispenser.
The line was rejecting parts on optical inspection, not on cure. Yield was limited by the optical result, so increasing dispense accuracy or extending cure time could not recover it: the formulation had to be optically clean first.
That ordering matters. A scattering source inside the compound cannot be corrected downstream by dispensing, and a clear liquid before cure is not evidence of a clear solid afterwards.
The solution.
GZ-5 high-RI catalyst with GZ-612 inhibitor; vacuum defoaming before dispensing to remove entrained air.
The process step matters as much as the grade: a soluble catalyst and a defoamed compound are both required before the transmittance number is meaningful, which is why the two changes were trialled together.
The trial used 4,000 PPM catalyst. Dosage was not the variable under test — compatibility was — so the loading was held at the value the customer's formulation required and changed only if cure was incomplete.
The result, and what produced it.
The numbers at the top of the page are the headline metrics from this case. The paragraphs here explain what produced them, with the test method and the exposure stated alongside.
Cured coupons measured 99.82% light transmittance and production yield reached 95%. Transmittance was measured on cured coupons using the customer's optical method, not on the liquid compound.
Read the result as compound-plus-process: solubility from the catalyst, air removal from defoaming. Remove either change and the number should be expected to move.
A change of dispense profile, vacuum level or compound batch is a reason to re-measure transmittance. The figure should not be transferred to a different optical stack.
Customer line trial, 4,000 PPM catalyst plus vacuum defoaming; transmittance measured on cured coupons per customer optical method.
Customer production case, published with permission.
The grades and the application behind this case.
Every case is tied to a catalyst grade and to an application page. The grade page carries the full specification; the application page carries the process window, dosage range and inhibitor pairing for this class of part.
| Model | Pt concentration | Viscosity | Recommended dosage |
|---|---|---|---|
| GZ-5 | Custom (1,000–20,000 PPM) | 400–800 cP | 0.05%–0.5% of total compound |
Open a model for packaging, shelf life, features and inhibitor pairing. Where a case names more than one grade, the solution section states which one was used in the reported trial.
Optical & Electronics
Refractive index above 1.50, zero haze.
High-refractive-index catalysts for Mini LED encapsulation, optical bonding and electronic protective films.
Other problems, measured the same way.
Each case is structured identically, so the challenge, solution and result can be compared across industries with the same reading discipline.
Battery pack seal: VOC compliance without losing compression set
A battery pack seal was built on a peroxide cure system. VOC emissions failed the customer's incoming specification, and the alternative addition-cure trial produced uneven cell structure and compression set above the 10% limit.
Medical LSR diaphragm: 100 steam cycles without yellowing
A respiratory valve diaphragm had to survive repeated 121°C wet-heat sterilisation without visible colour change. With the incumbent catalyst, yield after sterilisation was 82% and rejected parts were discoloured.
MLCC release film: 15-minute cure, +12% yield
The coater could not reach the surface roughness target of 0.2 μm at production speed because the silicone layer was not fully cross-linked when the film was wound.
Run a comparable trial on your own line.
Send the part, the failure and the acceptance test. We will send evaluation samples of the grade used in this case, paired with the matching inhibitor, and confirm the starting dosage for your cure window.