Technical / Highlights

The numbers behind a stable cure.

Three measurements separate this range from a standard Karstedt's catalyst: colour change after accelerated aging, activity retained after high-temperature exposure, and long-term stability above 150°C. Each is stated with its test conditions, because a number without a method is only a claim.

Measured performance

Three values that decide whether a line runs.

Accelerated colour aging, high-temperature activity retention and long-dwell thermal stability — each tied to a grade you can trial.

ΔE 0.8
Colour change after 85°C / 48 h

PC-42, measured against 4.2 for a conventional catalyst in the same run. Lower is better.

92%
Activity retained after 800°C

Core-shell design shields the platinum centre during high-temperature exposure, measured against an unexposed reference.

>150°C
Long-dwell stability, PC-50 / PC-51

For thick sections and hot-running parts, at 5–50 cP for even dispersion before gelation.

Side by side

PC-42 against a conventional catalyst.

Same substrate, same cure window, same test run — one catalyst changed.

PropertyConventional Karstedt's catalystPC-42
Colour change after 85°C / 48 hΔE 4.2 — visible to the eyeΔE 0.8 — within measured tolerance
Colour below 100°C, long dwellNot specified for colour-critical coatingHolds colour through long dwell times
PPF top coat, ΔE acceptanceFails a measured colour criterionSpecified grade for PPF top coats
Phenyl and high-RI systemsCan cloud the compound or drop out of solutionSoluble at typical loadings, optical clarity
Catalyst dosageCarried over from the incumbent formulation0.05%–0.5% of total compound
Recommended inhibitorFormulation-specificPC-611, PC-612 or PC-617

Typical results on reference formulations. Confirm the acceptance criterion for your own substrate and colour measurement method before specifying.

Four mechanisms

Why the range behaves differently.

Each differentiation changes what the platinum centre does under stress, not the marketing tier.

Anti-yellowing

Yellowing is an oxidation pathway that accelerates as a compound sits at temperature. PC-42 holds colour below 100°C for long dwell times, and at 85°C for 48 hours it measures ΔE 0.8 against 4.2 for a conventional catalyst in the same run. That gap keeps a top coat inside a measured colour specification.

Heat resistance

PC-50 and PC-51 remain stable above 150°C in long-dwell service. PC-51 also lifts the heat resistance of the compound: methyl silicone moves toward phenyl-level performance, phenyl toward fluoro. Both are low viscosity at 5–50 cP, so they disperse evenly in thick sections.

Anti-poisoning

Sulfur, phosphorus and nitrogen traces on substrates deactivate a platinum catalyst before cross-linking is complete. PC-18B is the production grade for slight to moderate contamination. PC-18A targets high concentrations and multiple contaminant types; it is under final R&D, with evaluation samples only.

High refractive index

In phenyl systems an ordinary catalyst can cloud the compound or precipitate out. GZ-5 is fully soluble with refractive index above 1.50, zero turbidity and zero precipitation. In a Mini LED encapsulation trial it supported 99.82% light transmittance at 95% yield.

How it is measured

Test conditions, not marketing conditions.

Colour aging runs on coated coupons at 85°C for 48 hours, with ΔE measured against an unstressed reference. The comparison catalyst is included in the same run, so temperature drift affects both equally.

Activity retention exposes a sample to 800°C, then re-tests it against an unexposed reference. Thermal dwell tests run PC-50 and PC-51 above 150°C in thick sections, where the centre of the part cures later than the surface.

Where a property has not been measured, the TDS describes the mechanism instead of quoting a number.

Ask for the method

Every value comes with four attachments.

  • Test method and reference formulation
  • Grade and dosage used in the comparison
  • Inhibitor pairing and cure window
  • Corresponding TDS revision
Technical FAQ

Questions the data raises.

Are these figures guaranteed specifications?

No. They are typical results on reference formulations, published so you can judge whether a grade is relevant. Guaranteed limits belong in the quotation and supply agreement, not on a product page.

Which grade should I try for yellowing?

PC-42 is the starting point below 100°C. If the part also sees long dwell above 150°C, start with PC-50 or PC-51 and confirm the inhibitor pairing for your cure window.

What does 92% activity after 800°C mean?

It describes how much activity survives a controlled 800°C exposure and quantifies the protective effect of the core-shell structure. It does not mean a finished compound can run at 800°C; the long-dwell claim is stability above 150°C.

Where can I see the full test conditions?

The TDS for each grade states the method and the reference formulation alongside the value. Test reports can be requested with a sample or a quotation, starting from the downloads page.

Where to go next

From a number to a trial.

Reading a specification is the first step; the useful step is a cure run in your own lab, with your own substrate and acceptance criterion. Evaluation samples are available for every grade, and the paired inhibitor ships with the catalyst.

Samples ship in 5–7 days with COA, TDS and SDS. Technical reply within 24 hours.

Next step

Put the numbers against your own acceptance criterion.

Send the colour, heat or contamination problem you are solving, with your cure window and substrate. We will reply with a suggested grade, starting dosage and the documents to run a comparison in your own lab.

Technical reply within 24 hours
Evaluation samples in 5–7 days
COA, TDS and SDS on request
Custom concentration 1,000–20,000 PPM